This age hardenable nickel base super alloy has very good strength in temperatures up to about 980°C (1800°F). It’s strength is generally comparable to that of Rene 41 and is generally superior to that of Alloy 718 at temperatures exceeding 650 – 705°C (1200 – 1300°F).
Click to find out more about each profile type.
.001” (0.025 mm) Diameter
.827” (21 mm) Diameter
Available in coils, spools and straight bars.
.0015" (0.3mm) Diameter
.787" (20mm) Diameter
Available in coils, spools and straight bars.
.0157" (0.4mm) Diameter
.394" (10mm) Diameter
Available in coils, spools and straight bars.
Specifications
Designations
Heat Treatment of Finished Parts | |||||
---|---|---|---|---|---|
Condition as supplied by Alloy Wire | Type | Temperature | Time (Hr) | Cooling | |
°C | °F | ||||
Annealed | Stabilize Age Harden |
843 760 |
1550 1400 |
4 16 |
Air Air |
Spring Temper | Anneal Stabilize Age Harden |
1050 843 760 |
1920 1550 1400 |
4 24 16 |
Air Air Air |
Condition | Approx. tensile strength | Approx. operating temperature depending on load^^ and environment | ||
N/mm² | ksi | °C | °F | |
Solution Annealed | 800 – 1100 | 116 – 159 | – | – |
Solution Annealed + Aged | 1300 – 1500 | 189 – 218 | up to +550 | up to +1020 |
Spring Temper | 1300 – 1600 | 189 – 232 | – | – |
Spring Temper + Annealed + Aged | 1300 – 1500 | 189 – 218 | up to +550 | up to +1020 |
▲ Dynamic applications = active / lively / changing